Alloy X is a high temperature and corrosion resistant nickel-base solid solution strengthened alloy. This alloy has outstanding resistance to oxidation at high temperatures and possesses exceptional strength at elevated temperatures. Alloy X exhibits good formability, weldability, and machinability.

Also know as Hastelloy X a registered trademark of Haynes International, Inc., Special Metals INCONEL® Alloy HX, Simalloy HX, Unitemp HX, Pyromet 680

Applications

gas turbine engine, Combustion liners, Turbine exhaust components, Aircraft cabin heaters, Transition Ducts

Specifications

UNS# N06002
5390D INVESTMENT CASTINGS
5536L SHEET STRIP & PLATE
5587D SEAMLESS TUBING
5588E WELDED TUBING
5754K BARS, FORGINGS & RINGS
5798D WELDING WIRE
B-366 FACTORY-MADE WROUGHT NICKEL & NICKEL ALLOY WELDING FITTINGS
B-438 PLATE, SHEET & STRIP
B-572 RODS
B-619 WELDED NICKEL & NICKEL-COBALT ALLOY PIPE
B-622 SEAMLESS NICKEL & NICKEL-COBALT ALLOY PIPE & TUBE
B-626 WELDED NICKEL & NICKEL-COBALT ALLOY TUBE
B-751 GENERAL REQUIREMENTS FOR NICKEL & NICKEL ALLOY WELDED TUBES
A-A-51173 (ERNiCrMo-2 ) RODS & ELECTRODES, WELDING, BARE
QQ-R-571C NICKEL ALLOY WELDING RODS
A5.14 SPEC. FOR NICKEL & NICKEL ALLOY BARE WELDING ELECTRODES & RODS
MR0175 SULFIDE STRESS CORRISION CRACKING RESISTANT METALLIC MEATERIALS FOR OIL FIELD EQUIPMENT
J467 SPECIAL PURPOSE ALLOYS ("SUPERALLOYS")
J470 WROUGHT NICKEL & NICKEL-RELATED ALLOYS

Available Forms

  • Bar
  • Coil
  • Fittings & Flanges
  • Forge
  • Investment Casting
  • Pipe
  • Plate
  • Sheet
  • Strip
  • Tubes
  • Wire